Properties
- Quickly levelling and brightening, the coating is full and bright, flexible, easy to be chrome plated.
- Get brightness at LCD, good throwing power, high impurity tolerance.
- Stable plating solution, convenient operation, low consumption, long big treatment processing period and strong corrosion resistance.
- Suitable for advanced plating of plumbing, plastic parts, electric fans, auto parts and motorcycle parts, especially suitable for fast nickel and multi-layer nickel process.
Operating Instruction
Formula and Operation Condition | Range |
Nickel Sulfate (NiSO4·7H2O) | 180~250 g/L |
Nickel Chloride (NiCl2·6H2O) | 45~55 g/L |
Boric Acid (H3BO3) | 45~55 g/L |
Nickel DM 880A brightener | 0.2~0.4ml/L |
Nickel DM 880B carrier | 6~10ml/L |
Y1 wetting agent | 1~2ml/L |
PH | 3.8~4.5 |
Temperature | 50~60℃ |
Cathode Current Density | 2.5~8.0A/dm2 |
Anodic Current Density | 1.0~3.0A/dm2 |
Filtration | Continous recycle filter |
Agitation | Cathode moving or air agitation |
Consumption
Additive |
Consumption |
Nickel DM 880A brightener |
150~250ml/KAh |
Nickel DM 880B carrier |
150~250ml/KAh |
Y1 wetting agent |
20~50ml/KAh |
Tank Transfer
It is easy to change the other nickel process to Nickel DM 880 fast nickel process. Stop adding previous brightener and carrier, replenish the make up amount as the previous tank or add Nickel DM 880 A and B at the ratio 1:1.