logo
Wuhan Fengfan International Trade Co.,Ltd. 86-27-85615818 info@fengfan.net
KCR-25 Chrome Plating Brightener with Fast Deposition Speed Chloride-Free Formula for High Micro-Hardness Hard Chromium Plating

KCR-25 Chrome Plating Brightener with Fast Deposition Speed Chloride-Free Formula for High Micro-Hardness Hard Chromium Plating

  • Destacar

    Fast Deposition Speed Chrome Plating Brightener

    ,

    Chloride-Free Hard Chromium Plating Additive

    ,

    High Micro-Hardness KCR-25 Brightener

  • Item
    Agente auxiliar químico
  • Tipo
    Brilhante de cromagem
  • Características
    Grade Industrial
  • Modelo
    KCR-25
  • Lugar de origem
    CHINA
  • Marca
    FENGFAN
  • Número do modelo
    KCR-25
  • Quantidade de ordem mínima
    Negociável
  • Preço
    Negociável
  • Detalhes da embalagem
    Embalagem de exportação padrão
  • Tempo de entrega
    15-25 dias de trabalho
  • Termos de pagamento
    L/C, D/A, D/P, T/T, Western Union, MoneyGram
  • Habilidade da fonte
    200000pcs/dia

KCR-25 Chrome Plating Brightener with Fast Deposition Speed Chloride-Free Formula for High Micro-Hardness Hard Chromium Plating


KCR-25 Hard Chrome Plating Chemicals Brightener High Cathode Efficiency


1. Properties


1. With high cathode efficiency, it may be up to 23%-26%.


2. The current density even over 60A/dm2 is available.


3. The deposition speed for KCR-25 bath is 2-3 times faster than conventional hard chromium process.


4. It is chloride-free, the KCR-25 process dose not cause erosion of the workpiece in low current density area.


5. The micro-hardness of the plating is up to 950HV-1100HV100.


6. The amount of the micro cracks of the plating may be up to 400/cm, so it improves the corrosion resistance ability of the plating.


2. Bath composition & Operation condition



Operation range

Standard

Chromium trioxide

200~275g/L

250g/L

KCR-25 Catalyst


20ml/L

Sulfuric acid

2.5~4g/L

2.7g/L

Temperature

50~60℃

58℃

Cathode current density(Dk)

50~75A/dm2

60A/dm2

Anodic current density

15~30A/dm2

30A/dm2



3. Reference Data


1. Deposition rate


Current Density (A/dm2)

Deposition rate (μm/h)

30

20-35

45

40-50

60

50-70

7.5

70-90


2. Bath density and concentration of chromic anhydride control



Chromium trioxide


Bath density

Baume degree (15)

Baume degree (60)

180

1.13

16.7

16.7

195

1.14

17.8

15.9

210

1.15

18.9

17.0

225

1.16

20.0

18.1

240

1.17

21.1

19.1

255

1.18

22.1

20.1

270

1.19

23.2

21.0

285

1.20

24.2

21.9

300

1.21

25.2

22.7